Grinding behavior and surface appearance of(TiC_p+ TiB_w)/Ti-6Al-4V titanium matrix composites

Ding DingWenfengZhao ZhaoBiaoXuJiuhuaYangChang-Yong

2014Acta Scientiarum Naturalium Universitatis SunyatseniEngineering被引 3

出版方页面 →

摘要

(TiCp+ TiBw)/Ti-6Al-4V titanium matrix composites(PTMCs) have broad application prospects in the aviation and nuclear field. However, it is a typical difficult-to-cut material due to high hardness of the reinforcements, high strength and low thermal conductivity of Ti-6Al-4V alloy matrix. Grinding experiments with vitrified CBN wheels were conducted to analyze comparatively the grinding performance of PTMCs and Ti-6Al-4V alloy. Grinding force and force ratios, specific grinding energy, grinding temperature, surface roughness, ground surface appearance were discussed. The results show that the normal grinding force and the force ratios of PTMCs are much larger than that of Ti-6Al-4V alloy. Low depth of cut and high workpiece speed are generally beneficial to achieve the precision ground surface for PTMCs. The hard reinforcements of PTMCs are mainly removed in the ductile mode during grinding. However, the removal phenomenon of the reinforcements due to brittle fracture still exists, which contributes to the lower specific grinding energy and grinding temperature of PTMCs than Ti-6Al-4V alloy.

引用本文(GB/T 7714)

Ding Ding, Wenfeng, Zhao Zhao, 等. Grinding behavior and surface appearance of(TiC_p+ TiB_w)/Ti-6Al-4V titanium matrix composites[J]. Acta Scientiarum Naturalium Universitatis Sunyatseni, 2014.

引文网络

参考文献与被引分析加载中…

本站仅收录题录与摘要供学习参考,全文版权归属出版方;如有侵权请联系我们删除。