The fibrous nickel oxide particles were prepared by chemical precipitation and pyrolysis method.TheNiO precursors were firstly precipitated from nickel ions solution with addition of oxalate salt,and then the finalNiO particles were obtained by pyrolysis of the precursor.The effects of the pH value,precipitation temperature,reactant concentration,addition of surfactant on the morphology of the precursor particles were investigated.Thecrystallinity,purity,morphology of the fibrous NiO were analyzed by XRD and SEM.The fibrous NiO particleswith 100-120 in axis/diameter ratio may be produced under the optimal process conditions that are proposed:theNi2+ concentration is 0.5-0.8 mol/L,pH value is 8.3-8.9,precipitation temperature is 60-75℃,pyrolysis temperature is 500-600 C.

引用本文(GB/T 7714)

张传福, 湛菁, 邬建辉, 等. Preparation of fibrous nickel oxide particles[J]. Acta Scientiarum Naturalium Universitatis Sunyatseni, 2003.

引文网络

参考文献与被引分析加载中…

本站仅收录题录与摘要供学习参考,全文版权归属出版方;如有侵权请联系我们删除。