Preparation of Porous Calcium Phosphate Bioceramic
摘要
Porous calcium phosphate ceramics were prepared by slip casting and molding method respectively. By these two different methods, different microstructures can be got. By slip casting method, the pore size was 100-350 μm and 20-80 μm; pores were opened, interconnected and ball-like; the grain size was 2-4 μm.By molding method, the pore size was 100-500 μm and 1-10 μm; the grain size was 2-8 μm. By slip casting method regular and interconnected pores can be got. By molding method the porosity and strength can be adjusted easily.